Hi,
Im trying to pattern su-8 on glass (square, rectangular slides). Edge bead seems
to be inevitable. Suggestions on minimizing them would be really appreciated.
thanks, krishna

````````````````````````````````````````````````````````````````````````````````
`````````````````````````````````````````````````
Krishna Vummidi

GRA, Wireless Microsystems Lab (www.ece.vt.edu/wml)
The Bradley Department of Electrical and Computer Engineering
Virginia Polytechnic Institute and State University
433 Whittemore Hall (Mail Code 0111), Blacksburg, VA 24061

(540) 231-3411 (Voice) -3362 (Fax)        E-mail: [email protected]

````````````````````````````````````````````````````````````````````````````````
`````````````````````````````````````````````````

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Nano-Master, Inc.
University Wafer
Process Variations in Microsystems Manufacturing