MEMSnet Home: MEMS-Talk: problems with gold plating
problems with gold plating
2004-10-06
Robert Dean
2004-10-10
IGOR KADIJA
2004-10-12
Josef Kouba
2004-10-07
Gary
problems with gold plating
Josef Kouba
2004-10-12
what you describe seems to be contaminated Au solution, I would suggest
replacing it with a new one and making sure you do not contaminate it again.


J.Kouba