MEMSnet Home: MEMS-Talk: 1050 °C for SU8
1050 °C for SU8
2004-11-04
Bruno Wacogne
2004-11-04
Hong Wu
2004-11-04
Christopher Blanford
2004-11-04
Thomas Hudgins
2004-11-05
Pierre Huet
1050 °C for SU8
Bruno Wacogne
2004-11-04
Dear all,

I have SU8 deposited on pure SI and I would like to oxidise the SI. For
this, I plane to make the oxidation with the following parameters: 1050 °C
in wet oxygen. Does anyone know if the SU8 layer will survive to this
treatment ?

Thank you for your answers,

Bruno


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing