RE: nickel etchants
2004-11-08
Michael Marrs
RE: nickel etchants
Michael Marrs
2004-11-08
Federico-

Transene has a pretty good nickel etchant. Here is a link to Transene's web
site:

http://www.transene.com/ni_etchant.html

Regards,

Michael Marrs
Process Engineer
Trion Technology
+1 (480) 968-8818 ext. 25
[email protected]