Aashish Singh
PMMA spin coating query
Aashish Singh
2004-12-22
  As a part of our project we need to spin coat a thin film of PMMA over quartz
block.
  Recently while searching on the internet i came across your reply to one
fellow on MEMS messaging regarding spin coating of PMMA.
  Is there  any empirical relationship between the film thickness (D), the spin
speed (w), the concentration of the polymer solution (C), and the molecular
weight of the polymer(M).
  Can anybody provide me with this relation and any references  suggested for
reading regarding spin coating of PMMA.
Your help will be heartly appreciated.

regards
Aashish singh
Project Associate
Department of Physics
Indian INstitute of Technology, Delhi
New Delhi
INDIA

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering