TaN
2005-01-11
Mojgan Daneshmand
2005-01-11
Neal Ricks
2005-01-12
Mahavir Sanghavi
2005-01-12
Mojgan Daneshmand
2005-01-12
Neal Ricks
Re:TaN
2005-01-14
Damiano Galvan
TaN
Mahavir Sanghavi
2005-01-12
Mojgan,

I had success in depositing TaN films using sputtering . Use lift off
process for TaN, etching TaN is not the way to go.

hope that helps,
-Mahavir Sanghavi