MEMSnet Home: MEMS-Talk: plasma-etching of fused silica
plasma-etching of fused silica
2005-01-17
Marlene
2005-01-17
Parijat Bhatnagar
2005-01-18
Marlene Brod
2005-01-18
Kirt Williams
2005-01-18
[email protected]
plasma-etching of fused silica
Marlene
2005-01-17
Dear All,

I am looking for any specific information about RIE-, ICP- or ECR-
etching of fused silica.
Which gasflow-rates, pressures, BIAS, temperatures... do you use?

I would be very happy if you could provide further assistance!

Yours, Marlene




reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing