MEMSnet Home: MEMS-Talk: su-8 ahesion
su-8 ahesion
2005-01-18
Xin Liu
2005-01-18
Bruno Wacogne
2005-01-18
Sonia Garcia Blanco
2005-01-18
Nicolas Duarte
su-8 ahesion
Xin Liu
2005-01-18
I'm working on fabricating SU-8 microstructures on glass slides,
it turns out that the adhesion of SU-8 on glass is poor. Does anybody
know how to solve this problem?

Thanks

Xin Liu

reply