MEMSnet Home: MEMS-Talk: RIE of GaAs
RIE of GaAs
2005-01-30
Guo, Wei
2005-01-31
fabio quaranta
RIE of GaAs
Guo, Wei
2005-01-30
Hi all,

I wanna etch the SiO2 on GaAs substrate by CF4 under RIE. I wonder
whether there is anyone know whether the CF4 etch the GaAs too. Thanks

Wei
reply