MEMSnet Home: MEMS-Talk: Preventing PDMS to PDMS bonding
Preventing PDMS to PDMS bonding
2005-02-15
Matthew Davies
2005-02-15
Bill Moffat
dryetch Al selectiv to Si
2005-02-17
Benjamin Voelker
Preventing PDMS to PDMS bonding
Bill Moffat
2005-02-15
Matt,
        I may have a possible answer.  I am working on super hydrophobic
surfaces that prevent any stiction.  I could run a trial through our system with
a hydrophobic chemical if you can mask the device so the areas you do not want
to stick are uncovered.  Contact me at [email protected]   Bill
Moffat

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
The Branford Group
MEMStaff Inc.