MEMSnet Home: MEMS-Talk: Re: "Mousebites"
Re: "Mousebites"
1998-04-03
Alexander Hoelke
1998-04-03
Jose Senna
Re: "Mousebites"
Jose Senna
1998-04-03
 Funny you mentioned it.
Recently these " mousebites started appearing in our lithography too.
I have a suspicion,I hope to test the hypothesis one of these days:
I think we are getting little droplets of water in our Nitrogen line.
Since we often blow dry the samples with N2, even AFTER priming, these droplets
may be giving origin to
poor adhesion in localized spots.

Simple tests: 1) Blow dry sample and check under microscope, and look for
droplets.
        2) Skip any blow drying, use only spin dry, and se if that gets rid of
mousebites.

Jose Rberto Senna
LAS-INPE
CP 515
12201-970 Sao Jose dos Campos SP
BRAZIL


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Addison Engineering
Tanner EDA by Mentor Graphics