"oxide balls" formation due to laser recrystallization
2005-02-21
Vinayak Shamanna
"oxide balls" formation due to laser recrystallization
Vinayak Shamanna
2005-02-21
i have laser recrystallised 0.5 microns of polysilicon on 0.4 micron thick
silicon nitride layer. I had sputtered these layers. instead of grains , i
got these oxide balls. i am not sure, why or how they are formed and is
there anyway i can get rid of them.
            Thank you
                                               regards,
                                               Vinayak Shamanna



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing