MEMSnet Home: MEMS-Talk: selective wet etching of Si with ZnO
selective wet etching of Si with ZnO
2005-02-18
Christiane Rieger
2005-02-23
David Springer
selective wet etching of Si with ZnO
David Springer
2005-02-23
Hi Christiane

Is there a reason why it has to be a wet etch. You could use Xenon Difluoride
gas (a dry process, no plasma) which will etch the silicon but not attack the
ZnO layer. If you would like to try it I can arrange for a couple of samples.

Regards
David Springer