measuring the deflection of a membrane
Burkhard Volland
2005-02-28
>    everybody! I want to measure the deflection of a membrane, and the
magnitude of the deflection is about 30um.
>
>    Could you give me some advice on the work?

Read the articles by Artur Degen, University of Kassel, in J.Vac.Sci.Technol
or Microelectronic Engineering or other journals.

Best regards

B.E. Volland


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Tanner EDA by Mentor Graphics