> Date:          Thu, 2 Apr 1998 19:43:31 -0600 (CST)
> From:          Stefano Ratti 
> Subject:       Yttrium oxide emissivity
> To:            [email protected]
> Reply-to:      Stefano Ratti , [email protected]

> Does anyone know what the emissivity of the yttrium oxide is ??
> It should be temperature dependent. Does anyone have something like a
> table with the values of the emissivity at different temperatures??

We own an Agema 900 thermographic system with microscope lens which
we often use for thermal characterization of microsystems.
Experience has shown that tabulated values of material emissivities
are hardly usable in practice. As you may find in literature, various
kinds of emissivity are defined and what you need uses to be a
mixture of several values. It is therefore better to calibrate your
system well and calculate the emittance. If you like, we can try to
support you with our system.
Yours sincerely, Kai Hiltmann

mailto:[email protected]    http://www.IMIT.Uni-Stuttgart.de
K. Hiltmann
c.o. IMIT
W.-Schickard-Str. 10
D-78052 Villingen-Schwenningen

Tel. ++49-7721-943-236
Fax  ++49-7721-943-210


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
The Branford Group
Tanner EDA by Mentor Graphics