MEMSnet Home: MEMS-Talk: Indium soldering
Indium soldering
2005-03-09
Zhiyan Liu
Steppr inside vacuum?
2005-03-09
Andrew Xiang
2005-03-10
David Nemeth
what stepper motor to do inside vacuum?
2005-03-10
Andrew Xiang
2005-03-09
Yu, Keven
Indium soldering
Yu, Keven
2005-03-09
Au will quickly diffuse into In, Au/In is a good choice at low temperature
bonding.

-Keven