A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: PDMS thickness variation with spin speed and time.
PDMS thickness variation with spin speed and time.
2005-03-15
Kapil Sahasrabudhe
2005-03-15
[email protected]
2005-03-15
Gary
2005-03-15
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
[email protected]
2005-03-16
Kapil Sahasrabudhe
2005-03-15
Z.,W.Y.(Lydia)
2005-03-16
karim faid
2005-03-17
Z.,W.Y.(Lydia)
PDMS thickness variation with spin speed and time.
Z.,W.Y.(Lydia)
2005-03-17
Hi, Karim,

The particles is also transparent. If you film thickness is match the particles
thinkness, just like you said 10-20um, you will not see this . I agree so sure.

If you are interesting in this , try to incerase the spin speed to 8K or higher,
I am sure you will see sth different. If not, please let me know.

Thanks,

Lydia

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation