MEMSnet Home: MEMS-Talk: coating a teflon layer on 8um glass spheres
coating a teflon layer on 8um glass spheres
2005-03-17
Yuejun Zhao
help..."stitch" two array together
2005-03-17
[email protected]
SUMMiT product line
2005-03-17
[email protected]
looking for recommendations
2005-03-17
[email protected]
2005-03-19
Natalya
coating a teflon layer on 8um glass spheres
Natalya
2005-03-19
Hi Zhao,

We have experience with hydrophobic (teflon-like) coating (FDTS) deposition
on fine powders from a vapor phase. It works well, no agglomeration of
particles during or after deposition is detected.

Boris Kobrin
Applied Microstructures
(408) 594-0654
[email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics