MEMSnet Home: MEMS-Talk: Alternative to AZP4620 and AZ400K
Alternative to AZP4620 and AZ400K
2005-03-21
Pete Kirby
2005-03-21
Giancarlo Corti
native oxide of aluminum film
2005-03-22
li cai
2005-03-22
Isaac Wing Tak Chan
Alternative to AZP4620 and AZ400K
Pete Kirby
2005-03-21
Hi-

Does anyone have an alternative to this combination with similar
performance? The staff here is complaining about the metal in the
developer.