MEMSnet Home: MEMS-Talk: Plasma etching with sloped sidewalls.
Plasma etching with sloped sidewalls.
2005-03-30
Bruce Altemus
2005-03-30
Isaac Wing Tak Chan
2005-03-30
Shane Arthur McColman
2005-03-30
Bruce Altemus
2005-03-30
Isaac Wing Tak Chan
2005-03-31
Robert Dean
2005-03-31
Wilson, Thomas
2005-04-06
[email protected]
Plasma etching with sloped sidewalls.
Robert Dean
2005-03-31
Hello,

I think refractive micro-optics companies use a gray-scale lithography
process to make micro-lenses and other finely controlled arbitrarily shaped
etched microstructures.  It might be worthwhile to consult one of them.

Sincerely,

Robert Dean
Auburn University

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
MEMS Technology Review
The Branford Group
Mentor Graphics Corporation