MEMSnet Home: MEMS-Talk: Cr as resistor
Cr as resistor
2005-04-19
Mojgan Daneshmand
2005-04-20
Shay Kaplan
2005-04-20
[email protected]
2005-05-09
Mojgan Daneshmand
2005-05-10
Behraad Bahreyni
Cr as resistor
Mojgan Daneshmand
2005-04-19
Hello everyone,

 I need to deposit a resistive layer for an RF circuit. My main circuit
is from gold and we use Cr as adhesive layer. I was wondering if I can
use this Cr layer as resistive layer for biasing the RF circuit?? I
looked on the web, it seems no one is using Cr as resistors and everyone
is using it in the form of a mixture.  I was wondering if any one has
any information in this regard that can help me??
Thanks everyone, it is really appreciated.
Mojgan


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
Tanner EDA by Mentor Graphics