MEMSnet Home: MEMS-Talk: Re: Rép. : [mems-talk] SU-8 Developing Issue, advice required
Rép. : [mems-talk] SU-8 Developing Issue, advice required
2005-04-20
Laetitia Philippe
Re: Rép. : [mems-talk] SU-8 Developing Issue, advice required
2005-04-20
Nan Xie
Re: Rép. : [mems-talk] SU-8 Developing Issue, advice required
Nan Xie
2005-04-20
Hello Laetitia,

I am using an I-line UV Lamp with attempts at 100 - 1000mJ/cm^2.

Nan
----- Original Message -----
From: "Laetitia Philippe" 
Subject: Rép. : [mems-talk] SU-8 Developing Issue, advice required

> Hallo Nan Sie
>
> I had the same problem and my answer was in the exposure time. which
> source you are using and how long do you expose?

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.