Hello everyone

I am trying to make an ohmic contact on the backside of a low doped Si(111).
The problem is that the sample should be heat up to 1100 C to form 7x7
pattern, This means ohmic contact should be stable at 1100 C. Usual
method to make an ohmic contact don't work for this because it is not
stable at high temperatures.

Does anybody know what kind of material I can use to form an ohmic
contact on backside for this temperature?

Thank You
Leo
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing