A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: TaN etching
TaN etching
2005-05-17
Hayashi Hidekazu
TaN etching
Hayashi Hidekazu
2005-05-17
Dear Sirs,

We are also looking for TaN etchant without silicon substrate and plasma-SiO2.
However, we won't be able to use alkali solution. We need acid etchant.
If you have any solution, could you please teach us soon?

regards,