MEMSnet Home: MEMS-Talk: Dielectric fill material for deep trenches
Dielectric fill material for deep trenches
2005-05-16
Bob Henderson
2005-05-17
[email protected]
2005-05-17
[email protected]
Surface Stress & Cantilever
2005-05-17
Sudhanshu Garg
2005-05-18
Oliver Horn
2005-05-18
[email protected]
Dielectric fill material for deep trenches
Oliver Horn
2005-05-18
Hello Bob,

we filled a similar trench with thermal oxide. If you could produce the
trench smaller, because the oxide grows  approximately half way in and
half way out. So if your trench could be 0.5 µm, this may work for you.
The upper edge gets normally round.

best regards,

Oliver Horn
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Mentor Graphics Corporation