Hi
I am exposing PMMA to higher doses so that it acts like a negative
resist. The final removal of PMMA can be done with oxygen plasma, but
it can damage my structure. So please suggest some other method other
than oxygen plasma to remove crosslinked PMMA effectively.
Thanks