high melting-point wax
2005-06-15
Mac Daily
2005-06-15
Minghai Li
high melting-point wax
Minghai Li
2005-06-15
why not try PMMA(950k) to stick your chip and it can stand at 80c.
On Wed, 15 Jun 2005, D. Zhou wrote:

> Does anyone know where I can get some high melting-point wax which can be
> used to stick the chip at a temperature of about 80 degrees? I tried black
> wax but it melt at 80 degrees. Many thanks.