eutectic point of silicon-aluminum
2005-08-12
Gary
2005-08-12
Scott Walck
2005-08-12
Bill Moffat
2005-08-14
rakesh babu
eutectic point of silicon-aluminum
Scott Walck
2005-08-12
I searched the internet and found a Silicon-Aluminum phase diagram.
Here is the URL:
http://www2.umist.ac.uk/material/research/intmic/phase/alsidiag.htm  The
eutectic composition is approximately 87 wt% Al and the eutectic
temperature is 660C.


-Scott

-----Original Message-----
From: Gary
Sent: Friday, August 12, 2005 10:46 AM
To: 'General MEMS discussion'
Subject: RE: [mems-talk] eutectic point of silicon-aluminum

Li, These materials don't truly alloy, hence there is no eutectic, The
"alloys" are really finely divided mixtures, and manufactured using an
atomization process.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMS Technology Review
Tanner EDA by Mentor Graphics