Hi Anwar:

For bulky silicon, the poisson's ratio is 0.22 - 0.27, thermal conductivity 1.3
W cm-1°C-1, Thermal expansion coefficient 2.6·10-6°C -1. Cannot find the value
of Jeta.

You may refer to http://www.memsnet.org/material/siliconsibulk/ and
http://www.ioffe.rssi.ru/SVA/NSM/Semicond/Si/index.html for more data and more
references.

Rgds,

Simon Xuming Zhang
Research Associate
School of Electrical & Electronic Engineering
Nanyang Technological University

Bill Moffat  wrote:
I do not know the eutectic point. I do know that in at least 5 different
semiconductor manufacturers I worked in we alloyed aluminum to silicon at about
435 degree C in a reducing atmosphere. It led to the manufacture of our 450
degree C oven with reducing gas control.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing
MEMStaff Inc.
MEMS Technology Review