+++ Pyrex wafer anodically bonded toThinSilicon:Problem +++
2005-08-23
Bill Moffat
+++ Pyrex wafer anodically bonded toThinSilicon:Problem +++
Bill Moffat
2005-08-23
Badin,
      What's wrong with plasma bonding.  Simply plasma treat the 2
surfaces and then place in contact.  The surface bonds are disturbed by
the plasma, then placing in contact the bonds interact with a merged
surface.  We have done dissimilar materials as well as identical
materials.


Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
MEMStaff Inc.
Mentor Graphics Corporation