Hello all:

I want to form a thin layer of oxidise on the surface of my silicon
wafer(20-50nm)
it is not easy for me to character the sample after oxidization.
is there anybody can tell me some recipe to do so?
such as temperature, time, oxigen pressure etc.

best

Yu Chen