MEMSnet Home: MEMS-Talk: Searching for a positive photoresist
Searching for a positive photoresist
2005-09-12
Sven Passinger
Searching for a positive photoresist
Sven Passinger
2005-09-12
Hi

I'm searching for a positive photoresist in which aliphatic hydrocarbons
are used (e.g. hexan or pentan).
I need this because I have a polycarbonate on which I want to bring
structures and this is only resistant against aliphatic hydrocarbons or
light acids.
Knows anybody such a resist or a supplier of this?

Thanks in advance
Sven
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Harrick Plasma, Inc.
MEMS Technology Review