Hello,

I'm trying to deposit a 0.5 micron layer of titanium/gold on a portion
of a PMGI mesa, but after the lift-off there are no metals left.
I use titanium only to improve the adhesion between metal and resin.
Note that the PMGI is previously baked at 230 °C for 5 minuts and
reflowed at 300 °C for 7 minuts.
I wonder whether anybody has an idea how I could increase the adhesion
between PMGI and metals.

Thanks !
Giuliano
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Addison Engineering
Process Variations in Microsystems Manufacturing