MEMSnet Home: MEMS-Talk: double-sided adhesise tape
double-sided adhesise tape
2005-10-20
Андрей Ткаченко
2005-10-20
Richard Chang
2005-10-20
GARCIA BLANCO Sonia
2005-10-20
Han G. Yoo
double-sided adhesise tape
GARCIA BLANCO Sonia
2005-10-20
Hi Andrey,

I have used it for mounting little parts in my supttering system. The
deposition was OK.

Regards,

Sonia.


-----Message d'origine-----
De : [email protected] [mailto:[email protected]]
Envoyé : Thursday, October 20, 2005 6:18 AM
À : [email protected]
Objet : [mems-talk] double-sided adhesise tape


 Hi,
It's common knowledge that double-sided adhesive tapes are used for dicing
and drinding. But I have heard about its application for evaporation or
sputtering as wafer mount. Has anybody such experiance? Would you mind to
advise anything about it?
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
University Wafer
MEMS Technology Review