A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: SiO2 hydrophilic enhanced?
SiO2 hydrophilic enhanced?
2005-11-07
Wullinger, Michaela
2005-11-07
Shay Kaplan
HD-8820 Polyimide
2005-11-07
Giuliano Gregori
2005-11-08
walter
2005-11-07
ssood
2005-11-07
sokwon Paik
Crosslink PMMA
2005-12-01
[email protected]
2005-12-02
Fabio Altomare
anodic bonding question
2005-12-02
Robert Dean
2005-12-03
Kirt Williams
2005-11-07
Gary
SiO2 hydrophilic enhanced?
Shay Kaplan
2005-11-07
Micahela,
HMDS will make it hydrophobic.
Plasma treatment might help.
shay

-----Original Message-----
From: Wullinger, Michaela
Sent: Monday, November 07, 2005 7:05 PM
To: [email protected]
Subject: [mems-talk] SiO2 hydrophilic enhanced?

hi all,
I'm thinking about ways to make SiO2 more hydrophilic.
What do you think about:
*HMDS?
*Temperature (heating)
*Other promoter?

Any hint is welcome
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review