one more wax question
2005-11-10
Abhinav Bhushan
2005-11-10
Brent Garber
2005-11-10
Ad Hall
2005-11-11
David Henriks
Process control
2005-11-11
jedidi nader
2005-11-12
PRAMOD GUPTA
Wet Etchant for silicon nitride
2005-11-20
Roger Brennan
2005-11-21
Carel Heerkens
EPON SU8
2005-11-21
Ladan Abolghasemi
2005-11-10
Adamson, Steve
one more wax question
Abhinav Bhushan
2005-11-10
Hi,

I want to use wax as a sacrificial material. I am
looking for one
which will melt at >100 C, preferably 125 C, and which
can be
dissolved in a solvent (acetone, hexane, etc). I was
wondering if
anyone has worked with or looked into a product like
this. I looked
online for wax, most of the ones available were used
for mounting
samples, I am not sure how clean the surface would be
after removing
the wax. The wax I have right now melts at 60 C, so I
cant use it the
way I want to. I will appreciate any help.

Thanks.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
University Wafer
Nano-Master, Inc.