Boris Kobrin
2005-11-18
Bill Moffat
RE: PTFE coating
Bill Moffat
2005-11-18
Pavel,
      Using specific silanes in our 1224 silane deposition equipment we
can exceed the contact angle of Teflon. Contact me for details of free
tests, details of chemistries used and specific details from our close
to 2,000 installations.

Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353

------------------------------

Message: 5
Date: Fri, 18 Nov 2005 08:00:39 +0100
From: Pawel Janus 
Subject: [mems-talk] PTFE coating
To: [email protected]
Message-ID: <[email protected]>
Content-Type: text/plain; charset=ISO-8859-1; format=flowed

Hi all,
I'm looking for PTFE coating provider. I'd like to deposit teflon on
silicon/silicon dioxide layer. I would be grateful for any information.

Regards
Pawel

_______________________________________________
Hosted by the MEMS and Nanotechnology Exchange, the country's leading
provider of MEMS and Nanotechnology design and fabrication services.
Visit us at http://www.mems-exchange.org

Want to advertise to this community?  See http://www.memsnet.org

To unsubscribe:
http://mail.mems-exchange.org/mailman/listinfo/mems-talk

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Addison Engineering
MEMS Technology Review
Nano-Master, Inc.