MEMSnet Home: MEMS-Talk: PDMS binding to GLASS
PDMS binding to GLASS
2005-11-19
suppi
2005-11-19
[email protected]
2005-11-20
karim faid
2005-11-21
Lee Pang
2005-11-21
Beggans Michael H IHMD
PDMS binding to GLASS
Beggans Michael H IHMD
2005-11-21
If you've got an ozone cleaner, it works the same as the plasma. About a
minute or two clean and then bond.

Mike

Dr. Michael H. Beggans
Naval Surface Warfare Center, Indian Head
101 Strauss Ave. Bldg. 302            Phone: (301) 744-1927
Indian Head, MD 20640                  Fax:    (301) 744-6406
-----Original Message-----
From: suppi [mailto:[email protected]]
Sent: Saturday, November 19, 2005 12:48 PM
To: [email protected]
Subject: [mems-talk] PDMS binding to GLASS

Hi all,

I want to irreversibly bind PDMS to Glass but do not have a plasma cleaner.
IS there any other method of doing it. PLease reply ASAP.

Thanks in advance.
Supriya

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
Process Variations in Microsystems Manufacturing
University Wafer
Tanner EDA by Mentor Graphics