MEMSnet Home: MEMS-Talk: Polyimide remove
Polyimide remove
Polyimide thinner
2005-11-19
Lung-hao Hu
2005-11-23
Lung-hao Hu
2005-11-23
[email protected]
2005-11-23
Michael D Martin
Polyimide remove
[email protected]
2005-11-23
If you have a downstream plasma using Oxygen you will not attack the gold
much. I would think chemical means would be worse since it might make the gold
lift. Bob Henderson