MEMSnet Home: MEMS-Talk: .3/.5 mm thick glass
.3/.5 mm thick glass
2006-01-01
gillot
2006-01-04
Jauniskis, Linas
.3/.5 mm thick glass
Jauniskis, Linas
2006-01-04
I have bought down to 0.2mm 4x4" sheets Schott borosilicate from S.I.
Howard Glass. They are pretty painless to work with, but maybe not if
you are outside the US. Shipping without breakage can be a challenge.

http://www.howardglass.com/D263.html

Linas.

-----Original Message-----
From: [email protected]
[mailto:[email protected]] On Behalf Of gillot
Sent: Saturday, December 31, 2005 10:14 PM
To: General MEMS discussion
Subject: [mems-talk] .3/.5 mm thick glass


Dear List,

Happy new year !

I am looking for plate glass with a thickness of .3 or .5 mm to be
sputtered, but it seems that it doesn't exist on earth...
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing