Dear,


I am trying to find appropriate polyimide either photodefinable or
standard to coat 20 micron of dielectric layer film. I'm mainly concerned
on the dielectric constant property to be around 3.3 to 3.5, and
resolution of at least 20 microns. Can anyone give me advices on the
selection of polyimides. Will photodefinalbe polymide be applicable for the
above specs?
Thank you.


Brandon
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
Mentor Graphics Corporation