Hello,

I am trying to fabricate a suspended aluminum (99% Al, 0.5% Si, 0.5% Cu)
structure, 1.15um thick on a silicon wafer.  The suspended length is
approximately 130um.  After the structure is released etched from the
silicon using XeF2, the aluminum bridge bows and twists due to stresses.
What causes this and how can I prevent it?  Thank you.

Sincerely,

Robert Dean
RF CMOS Designer
MEMS Optical
205 Import Circle
Suite 2
Huntsville, AL 35806
Tel. 256-859-1886
FAX 256-859-5890
email [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Addison Engineering
MEMStaff Inc.
Process Variations in Microsystems Manufacturing