MEMSnet Home: MEMS-Talk: Solderable metallization recipe on glass & ceramics
Solderable metallization recipe on glass & ceramics
2006-01-23
Jauniskis, Linas
2006-01-23
Peter Svasek
2006-01-23
sokwon Paik
2006-01-23
walter
optical profilometer
2006-01-23
[email protected]
2006-01-23
ssood
microscope lens
2006-01-24
li cai
2006-01-24
David Nemeth
Solderable metallization recipe on glass & ceramics
Jauniskis, Linas
2006-01-23
Could anyone suggest an evaporated metallization (metal layers &
thickness) recipe on glass & ceramics (alumina) that one can solder to
with SnPb 63/37 and SnAg 96.5/3.5 solders.
Thanks!
Linas.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing