capacitive accelerometer
2006-02-03
trinadh allaka
2006-02-05
g.balsubra manian
2006-02-06
Shile
capacitive accelerometer
g.balsubra manian
2006-02-05
yes. But You have to use Some metal as adhesive (seed
layer) inorder to fix electrodes..by metallization.,

Generally chromium is better..or Titanium.,

Then You can deposit the metal you want by
metallization..

Regards.,

Balasubramanian
Mcmaster university.


--- trinadh allaka  wrote:

> Hai all
>
> I am designing a capacitive acceleromete. My
> question is can I use metal
> layer as the interconnect to fixed electrodes and to
> feed excitation? Which
> metal layer is preferred?
>
> My fab flow is
>  wafer definition
> Deposit silicon nitride
> Deposit metal
> etch metal
> Deposit silicon dioxide
> etch siO2
> deposit polysilicon
> etch poly
> sacrifice  siO2
>
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing