MEMSnet Home: MEMS-Talk: dip-coating superhydrophobic coating
dip-coating superhydrophobic coating
2006-04-05
yilei zhang
2006-04-05
Matthew Coda
2006-04-05
Bill Moffat
dip-coating superhydrophobic coating
Bill Moffat
2006-04-05
Simple vapor prime with any of the high fluorine silanes. For example
(heptadecafluoro1,1,2,2,-tetrahydrodecyl)trichlorosilane can give you
contact angles of 130 degrees.  Teflon is only 120 degrees.  You need to
vacuum dehydrate then treat with heated silane vapors to achieve
surfaces that moisture does not attack. We have built specialized
equipment to do this for years. Test us free.


Bill Moffat, CEO
Yield Engineering Systems, Inc.
2185 Oakland Rd., San Jose, CA  95131
(408) 954-8353


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics
University Wafer