MEMSnet Home: MEMS-Talk: G-line for SU-8
G-line for SU-8
2006-04-07
Matteo Dainese
How do clean the Cr mask?
2006-04-07
[email protected]
2006-04-07
Brubaker Chad
G-line for SU-8
Brubaker Chad
2006-04-07
SU-8 is virtually transparent to g-line (effectively zero absorption of
wavelengths above 390 nm), and is non-reacting with it.

Best Regards,
Chad Brubaker


-----Original Message-----
From: Matteo Dainese
Sent: Friday, April 07, 2006 7:50 AM
To: [email protected]
Subject: [mems-talk] G-line for SU-8

Hello,
has anybody experience in exposing SU-8
using a g-line stepper (the only we can use)?
We would need to use thin films (<5µm) of SU-8
for making optical waveguides, but we found
no evidence in publications whether
the absorption would be enough for a
good exposure.
Thanks for your comments.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Harrick Plasma, Inc.