Hello ,

I am using Dry film MX5000 series from Dupont for lift off process on SU-8
2002 photoresist. I am finding it difficult to remove the dry film after
laminating on SU-8 2002 during the lift off process.

I am using Dynasolve PR 7200 dry film stripper.

Please let me know how to get rid of Dry film on SU-8 2002?

Suggestions would be appreciated.

Thanks.

--
Phaninder Reddy Kanikella
University of Missouri-Rolla
USA.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics