Wet etching Copper selective to Nickel
2006-04-14
Srinivas Vanapalli
Wet etching Copper selective to Nickel
Srinivas Vanapalli
2006-04-14
Hello All,

I have Nickel electroplated on Copper as a seed layer with photoresist as the
mask. I have to
remove copper at those areas where photoresist was mask during electroplating. I
am looking for
wet etching recipies selective to Nickel. If somebody has done this before pls
let me know. Thanks
in advance.

Srini.
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics