EDP Etching
2006-05-17
faizal
EDP Etching
faizal
2006-05-17
hi all..

i'm new in MEMS field..now i'm working on mems
micromachining using 'wet etch' to fabricate suspended
micstructure for thermal isolated devices (V shape).
So far we have KOH as an etchant (etch rate=very
slow). i've decided to vary the etchant like EDP. Any
good reference for this instead of Marc J.Madou's
books, plz share with us..
tq..

cheers

Mohd Faizal Aziz
Institute of Microengineering and Nanoelectronics (IMEN)
Universiti Kebangsaan Malaysia
reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering