MEMSnet Home: MEMS-Talk: Re: Looking for Polyimide suppliers
Re: Looking for Polyimide suppliers
1998-03-25
Shekhar Bhansali
1998-03-25
Eui-Hyeok(EH) YANG
1998-03-25
Ladislav Matay
Re: Looking for Polyimide suppliers
Ladislav Matay
1998-03-25
Try polyimide named PYRALIN from Du Pont:

Du Pont Co.,
P&EP Dept., EMD
Reynolds Mill Building
Barley Mill Plaza
Wilmington
DE 19898
USA

Tel: +1(800)441-7543


Ladislav Matay

Cheol-Hyun Han wrote:

> Hi;
> Does anybody know about the  ployimide which has good adhesion with Si and
> those suppliers?   In my case, adhesion is so important.   Any
> information would be welcome.
> Thanks.



--
LADISLAV MATAY
INSTITUTE OF COMPUTER SYSTEMS
SLOVAK ACADEMY OF SCIENCES
SK-84237 BRATISLAVA
SLOVAKIA
TEL: 00421.7.3782743
FAX: 00421.7.371004
[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
Nano-Master, Inc.
MEMStaff Inc.